Topic: Filament Pelletizer Version 2
Hi All,
I built a drill powered pelletizer similar to Ian's design and it worked well enough.
( Search Youtube for " Plastic Filament Pelletizer Powered By Drill ")
However, I was concerned about the metal to metal contact of cutting surfaces and
metal filing contamination. Here is the new design in action on Youtube:
(Search Youtube for " Plastic Filament Pelletizer v2 Powered By Drill)
It uses a standard 1" Forstner wood boring bit with a 3/8" shaft. It is supported
by two ball bearing bushings. No metal to metal contact on the cutting surfaces.
Bill