1 (edited by ggunners 2014-02-17 22:43:27)

Topic: Gyro The Cube print

This one was printed at 200 microns with supports (KISS) and took 14 hours and 34 minutes.

Clean up takes awhile and this was my 2nd attempt at the Gyro The Cube print. The first one was at 60% and it self destructed when removing the supports. I had sliced it with KISSlicer and used  a 20% infill. So, I decided it must be the infill and size, so I made it at 100% size with solid infill. Unfortunately, the sides split right along the horizontal layer lines on the most narrow section. I really don't think this one can be printed and survive with the SD2 ABS red I have.

That said, there's one here that says it is thicker, that I may try next. It's called the Big Thick Gyro Cube v2.

-- ggunners

http://www.soliforum.com/misc.php?action=pun_attachment&item=4656&download=0

Post's attachments

gyro-the-cube.jpg
gyro-the-cube.jpg 194.96 kb, file has never been downloaded. 

You don't have the permssions to download the attachments of this post.
SD2 Expert stock, ABS fume fan,
XYZ DaVinci 1.0 stock ABS, Simplify3D
QUBD Two-Up PLA, new 3D printed X gantry, Y idler, flex z coupler, extruder mount, E3D Lite

2

Re: Gyro The Cube print

Nice job smile

3

Re: Gyro The Cube print

nice job