1

Topic: 3mm filament???

So i bought 3mm filament by mistake... because I'm an idiot. Now i have a bunch of this laying around and was wondering if there are any upgrade i could print off to allow the larger filament? or should i just go buy 1.75mm and follow simple instructions like an adult? THANKS!

2

Re: 3mm filament???

your gonna need a new hot end  my friend, if you wanna print with 3mm.  cant you email your supplier and ask them if you can exchange it for 1.75? or maybe someone will trade you?

3

Re: 3mm filament???

Ya i was afraid of that and I just sent them an email hopefully i can just exchange it.

4

Re: 3mm filament???

where did you order from ?

5

Re: 3mm filament???

I got it from some place in Texas on good ole ebay. They claim they do returns but im just waiting on a reply so time will tell

6

Re: 3mm filament???

sounds like you should be alright. good luck!