tealvince wrote:Rocketman wrote:It seems like losts of people on here absolutely love using Acetone to smooth over models. Is there any proper way to dilute it down so that it may be used nearly with bare hands? I wouldn't mind if a print sat in it for a couple days.
I read that acetone can be diluted with water. There was a post a few weeks ago about a kickstarter campaign that used a water-diluted solvent bath circulated by a pump. If you go ahead and try it, please post your results. I personally think we should encourage new ideas rather than shooting them down.
I'm not shooting it down blindly. I'm just looking at it like this: We have a way to use a tablespoon of acetone in a $25 device to safely and effectively smooth our prints in a few minutes time. We're proposing a method of managing a diluted solution of acetone and water laying around for much longer, with a considerable amount of more effort, requiring more supervision, and likely costing more than the $25 device to setup. Once a simple solution is found I evaluate everything against that and it needs to improve in either cost, effort, time, safety, or results for it to be worth it for me. This doesn't seem to do any of that.