1 (edited by DesignerFred 2013-09-24 09:43:56)

Topic: Ancient communication tool, BullRoarer!

The DesignerFred BullRoarer smile

You never know when we might be using these again!!

http://thingiverse-production.s3.amazonaws.com/renders/46/01/72/f1/12/DesignerFredBullRoarers_display_large.jpg

http://www.thingiverse.com/thing:154046

http://en.wikipedia.org/wiki/Bullroarer_(music)

P.s. Use the included Handle for the large 100% model, or else blisters... And use in a safe place, never around people!

Post's attachments

DesignerFredBullRoarers.jpg
DesignerFredBullRoarers.jpg 458.88 kb, file has never been downloaded. 

You don't have the permssions to download the attachments of this post.
www.designerfred.fr      before: Solidoodle 2 + E3D v6 now: MeCreator II and OLO 3D

2

Re: Ancient communication tool, BullRoarer!

Any video of it in action? Do you print it 100% infill? How much does it weigh? Good work!

3 (edited by DesignerFred 2013-09-24 21:04:04)

Re: Ancient communication tool, BullRoarer!

Charles_Xavier wrote:

Any video of it in action? Do you print it 100% infill? How much does it weigh? Good work!

I printed with 100% infill, they both work well, the larger one 100% size is a bit heavy for beginners! I say start with the little one. I do not have a scale handy, but the handle is definately needed for the large size.

I used thin 1.5 mm synthetic string, they say thin line is best. Make sure your knots are well tied!! :° )

http://www.youtube.com/watch?v=3Kf_RYVt2XQ

Not mine but good video, notice the gloves and handle piece: http://www.youtube.com/watch?v=afaLL9BQv24

If I had to print the larger one again, I would try to lighten it to 60% infill.

Thanks, Enjoy!

www.designerfred.fr      before: Solidoodle 2 + E3D v6 now: MeCreator II and OLO 3D

4 (edited by DesignerFred 2013-09-25 20:30:25)

Re: Ancient communication tool, BullRoarer!

Ok.. here are my two videos... notice the large bullroarer is work! I will try a 75% scale size next!!

Small model video: http://www.youtube.com/watch?v=xXB7unDWVuw .......

Large model video: http://www.youtube.com/watch?v=HJeU-oTiw2c.....

and yes I look like a BullRoarer operator!

www.designerfred.fr      before: Solidoodle 2 + E3D v6 now: MeCreator II and OLO 3D

5

Re: Ancient communication tool, BullRoarer!

COOL!

6 (edited by DesignerFred 2013-09-27 12:28:02)

Re: Ancient communication tool, BullRoarer!

Thanks,

Ok, the 75% scale model sounds great, and is just right weight wise! I used the handle with it.

http://www.youtube.com/watch?v=Da448m55F7A

www.designerfred.fr      before: Solidoodle 2 + E3D v6 now: MeCreator II and OLO 3D