Topic: How would you make a hinge for this?
This is a battery compartment cover. It will be opened maybe a hundred times during the life of the product, which will be made of ABS unless someone can convince me otherwise.
I just made a thinner section you can see running under the BOLO logo, that would bend and hopefully not break during repeated bendings. BUT, it apears ABS has other ideas and wants to break sooner rather than later.
Space is at a premium, I don't want a bulky hinge or an ugly one. I think a magnetic one might interfere with electronics but maybe not, I'll experiment. I guess my question is, does anyone know of a single part hinge design like an accordion type or something that would print at this scale and resolution? Otherwise, how would you approach it?
Thanks, guys.