Topic: Creating textures to the 3d prints.
Hello.
I wanted my prints to have more than one color, so i experimented with few things and found a decent solution if you want to have a texture to your prints.
What you need is:
A Solidoodle!
Laser Paper Printer
Claudline Hellmuth - Studio Multi-Medium, Gloss(?)

So what you do is; Print out whatever you want using your 3D-printer. Design whatever logo\texture in your favorite design software (paint \ photoshop \ gimp etc). Then print it out using your Laser paper printer (Doesnt work with normal ink printers).
Then you put on some Claudline Hellmuth to the 3d printed object. After that you take the paper you printed out using your laser printer, and stick it to the claudline hellmuth that you put on your 3d print.
Make sure theres no air bubbles and then wait atleast 2-3 hours.
After the waiting game, put it all under wather and then carefully start to clean away the paper itself. Do it layer by layer and after few mins, the color will stick to the 3d printed object while the paper itself is washed away.
Here is my first experiement:

You can get the Claudline Hellmuth from here:
http://www.ellenhutson.com/servlet/the- … iate_no=17
Just google the name, and you can probably get it in your country aswell. :-)
I'm terrible at describing stuff, and making guides\tutorials isnt my thing, so give me some time and ill try update this enough so its understandable
- Atleast i found it pretty cool and easy to make more colors to your print.. Only bad thing is that you need a Laser printer, normal ink printer doesnt work as far as i know.
As i mentioned, this is my first test and i will be uploading more examples of how you can use it to make your 3d printed stuff to stand out more ![]()