Topic: Take a look at this bottom layer problem please.
Still limping along with my old extruder waiting on the E3D. My ABS bottom layer is real loose. In the pics maybe you can see that the infill is not physically connecting with the perimeters. when I turn the finished part over, the bottom is real coarse fill and has threads flying loose.
My corners are also lifting, despite 200C extruder temp, copious use of hair spray on glass, 100C bed temp and long warm up waits.
I have Searched here for a solution and piddled with various Slicer settings but, no cigar. Help please. Thanks.