Here is my first try with the software. I made the base layer .3 so it would be 1 layer, and the mesh is maybe 1.5mm. I would make it a little thicker next time. Also I would reduce contrast within the face a little more. There is a dark shadow along the side of her nose which makes that line deeper than it should be. I painted out any specular highlights, like in the eyes, and some glare on the lips. I figured those would get rendered as spikes and look odd.
Within the software I applied a fairly aggressive vignette to tone down the highlights from the beads in her hair.
Printed at .1mm. Not enough solid layers, or enough fill so there are a few gaps on the surface. Once I get a print that I like, I'll give it a run through the Presto Print Finisher (tm).
BTW, this is the kind of thing that can buy you more time on the printer without eye rolling, or grumbling about chores that need to be done.