Topic: Australian Suppliers for Borosilicate Glass
For use on glass beds this should really do the trick. Make sure you ask for 'Aras' glass, the supplier told me that just means they smooth the edges so you don't slice yourself open!
Anyway, I found these guys online. I have NO affiliation with them.
Glasslite Pty Ltd
1/40 Hi-Tech Drive
Toormina NSW 2452
Tel: 02 6658 5234
Fax: 02 6658 5240
Email: [email protected]
Website: www.glasslite.com.au
and the costs....
Thanks for your enquiry for the 200 x 214 x 3mm clear Borosilicate glass, prices are as follows -
Qty 1 $32.95 ea. + gst.
Qty 2 $22.60 ea. + gst
Qty 3 $19.15 ea + gst
Qty 4 $17.40 ea + gst
You'll have to enquire about shipping because it will vary depending on how much you order and where you are. I paid $19.95 for 4 sheets to Adelaide.
I will provide more feedback and info here after I've got my glass.