So, for the first time I tried producing colored filament. I mixed 200 g of MG94 granulate with 4 g of OS Printing's blue colorant and 4 g of yellow colorant (so 50:1:1 ratios). The goal was to produce green 3 mm filament.

The results... well, it looks much more awesome than I thought. Images attached.

Post's attachments

20130805-0152.jpg 81.73 kb, 1 downloads since 2013-08-06 

20130806-0153.jpg
20130806-0153.jpg 53.63 kb, 1 downloads since 2013-08-06 

You don't have the permssions to download the attachments of this post.