Topic: Warping on large print
Hi, i've just bought an SD2.
I've made few tries, but i've get warping issue on large box.
I've tried to clean klape with acetone, tried to get the SD more isolated, tried different temperature printbed (from 60 to 110).
But i've still get warping with 0.3 print after 50-60 layers (sometimes it happen later). Tried with different resolution (from 0.1 to 0.4, tried also to play with first layer speed)... (i've already set the Z axis)
Hard to find a good configuration.
I'm actually trying adding pad on my stl, but after few layers, two of the pad started warping .
I tried to add clothespin on the pad (the main structure -> a box) isn't warped yet.
Is there a way to stop warping with ABS on large print?