Http://fabbaloo.com/blog/2013/5/28/hands-on-with-the-finishingtouch-smoothing-station.html
Ok... now i need to add a fridge next to my crockpot vapor station... ![]()
You are not logged in. Please login or register.
SoliForum - 3D Printing Community → General Discussion → hands on stratasys smoothing station
Http://fabbaloo.com/blog/2013/5/28/hands-on-with-the-finishingtouch-smoothing-station.html
Ok... now i need to add a fridge next to my crockpot vapor station... ![]()
Liquid nitrogen dip before acetone smoothing, got it.
Will have to put some in the freezer for a half hour first next time... Fail to see how it would improve on the presto / rice cooker/ slow cooker though... Im done finishing a model within 5 mins of starting the acetone smoothing process...
30k sounds cheap tho
pffft
The cooling helps with getting the acetone to condense on the parts. I attempted to smooth some items outside on ahot day and got basically no smoothing, because the aceton did not condense on the parts. Will have to give the freezer a try.