1 (edited by LdyMox 2013-05-25 02:19:36)

Topic: Day 3- Faerie Bottle

Day 3 of a SD2 after clearing a nasty clog- Faerie Bottle. Transparent blue PLA. I should of added some support, some dropping at the bottom but otherwise nice looking.

http://www.soliforum.com/misc.php?action=pun_attachment&item=2156&download=0


Found it at http://www.thingiverse.com/thing:11121

Post's attachments

fariebottle2.JPG
fariebottle2.JPG 160.19 kb, file has never been downloaded. 

You don't have the permssions to download the attachments of this post.
Tammy
Solidoodle 2
E3Dv6 Hotend, MK5 v6 version, Glass Bed, Anti Z backlash slop nut, SureStepr SD8825 1/32 Extruder Driver, makeshift breakaway plexiglass case; . L-Cheapo 3.8 Watt Laser Attachment w/Custom built enclosure
From Buffalo, NY, USA

2

Re: Day 3- Faerie Bottle

Very cool! What software and settings are you using?

3

Re: Day 3- Faerie Bottle

I was just using the stock Repiter host&slicer and used the .3 profile. Since it was PLA put my extruder temp to 160 and my bed temp to 60.

Tammy
Solidoodle 2
E3Dv6 Hotend, MK5 v6 version, Glass Bed, Anti Z backlash slop nut, SureStepr SD8825 1/32 Extruder Driver, makeshift breakaway plexiglass case; . L-Cheapo 3.8 Watt Laser Attachment w/Custom built enclosure
From Buffalo, NY, USA

4 (edited by DesignerFred 2013-05-25 08:24:39)

Re: Day 3- Faerie Bottle

Very Nice, color too! I do PLA at 190° .... works great

www.designerfred.fr      before: Solidoodle 2 + E3D v6 now: MeCreator II and OLO 3D

5

Re: Day 3- Faerie Bottle

Well my clog happened at 180, I am thinking from the way it looked it got too soft and drooped. Maybe it is the enclosure. It does seem to run hotter then I set it usually. Even though I set it to 160 it often went to 165 or 170.

Tammy
Solidoodle 2
E3Dv6 Hotend, MK5 v6 version, Glass Bed, Anti Z backlash slop nut, SureStepr SD8825 1/32 Extruder Driver, makeshift breakaway plexiglass case; . L-Cheapo 3.8 Watt Laser Attachment w/Custom built enclosure
From Buffalo, NY, USA

6

Re: Day 3- Faerie Bottle

In case anyone was wondering about this fantastic blue color, as it almost shimmers.  I got it at http://www.amazon.com/3DPrintingUSA-Tra … B00BI1AHS0