1

Topic: Printing problems in the first layers

Hi guys, i'm having some problem when i try to print this piece (attachment)  after some layers is detached from the bed, i have problems only with this piece this is my configuration (attachment) is wrong for this type of print? Thanks for any type of help.

Post's attachments

config.png
config.png 43.15 kb, file has never been downloaded. 

superiore1.stl 22.31 kb, 17 downloads since 2013-05-12 

You don't have the permssions to download the attachments of this post.

2

Re: Printing problems in the first layers

Little up