Topic: 2009 Dodge Charger iPhone device
Hi all,
Below is a project I dd with my SolidDoodle on the Local Motors site (open source automotive design). It was really more of a learning exercise on a few things:
ABS (and warpage and rafting)
PLA.
Press fit and friction (or lack of friction with PLA)
Doing something practical instead of desk ornaments
Best design for overhangs
I need to better design the assembly to get a bit more rigidity but it basically works.
The project:
https://forge.localmotors.com/pages/pro … p?cg=11568
Finished product:

NX and Solid Edge CAD user
PI, Galileo, and arduino hacker
Code Monkey and Twitter user @burhop