wilheldp wrote:Does anybody have an engraver that can engrave metal trophy nameplates? If so, send me a PM...I'm in the market for one.
Question, do you really mean engraved and metal ? Because a lot of the 'metal' nameplates you see etc are actually Traffolyte panels, such as seen here: http://www.identitag.co.uk/engneering/T … labels.htm . I've seen quite a few trophy plates made up from Gold/Silver ones of this. This is lasercut or milled.
Or they are Brass/Aluminum using Laser Marking spray, such as LM Spray branded a "CerMark" : (Google Image Search: http://tinyurl.com/lvxfp8c ). These are just metals sprayed and then the LM Spray becomes indelible as a result of the laser striking it... you use it like a positive resist. These can give amazing results.. and you can get it in pressure-pack spray cans for one offs/small pieces to big fat vats for use in production lines.
Finally, there is baby CNC Engravers, which will 'mill' actual metal.. but their end result isn't nearly as nice as a good calligrapher with a wand-engraver when talking written engraving... Roland make some excellent jewellers mills and desktop engravers that can obviously do much better reliefs and the like than you could by hand..