1

Topic: 3D Ink

I had ordered clear, red and blue but my order was mixed up with someone else's and I received the clear, red and    two other colors I hadn't ordered.  I contacted 3D Ink about the mix up and they quickly sent my missing spool of blue abs.  I will be doing business with 3D Ink again.

2

Re: 3D Ink

can you tell us the link?

3

Re: 3D Ink

Have you looked at the clear yet?  Judging from the spool, it might be the same manufacturer as the one I got which had bubbles and contaminants.

4 (edited by ch355ma5t3r 2012-10-08 06:30:00)

Re: 3D Ink

Manx the link is http://www.buy3dink.com/

Ian the clear looks perfect, I couldn't find any specks or bubbles in it at all.  The dia is 1.77mm to 1.78mm from the 10ft of it that I checked. 
http://img272.imagevenue.com/loc361/th_673277462_CIMG1469_122_361lo.JPG

5

Re: 3D Ink

thanks for the link and interestign they have 3d resin to at a very nice price i wonder if its compatable with the form 1

6

Re: 3D Ink

The diameter on my clear was 1.55-1.66, and you could feel a little ripple.  Either it's a different supplier, or they got a better batch.  Either way, I'll probably order a spool from them since I'm afraid the one I have will clog my nozzle.

7

Re: 3D Ink

IanJohnson wrote:

The diameter on my clear was 1.55-1.66, and you could feel a little ripple.  Either it's a different supplier, or they got a better batch.  Either way, I'll probably order a spool from them since I'm afraid the one I have will clog my nozzle.

Have you had problems with bad filament from suppliers in the past?

Former Solidoodle employee, no longer associated with the company.