Topic: Extruder problems
Hi, I have not had a sucessfull print with my new SD3.
I was having sticking to the bed problems to start with
but after I changed the filament, that's the least of my problems.
I kept aborting the prints because nothing was sticking and I started to notice that the abs that was coming out was very thin and pink.
I had replaced the stock red with white.
Today I finally drew a sharpie line on the filament and realized it wasn't really moving.
So I tightened down the pressure screw on the wheel drive and the filament started bunching up in the print head.
So I stopped the printer. Removed the filament and cut a clean section then fed it back into the extruder.
That seemed to fix the problem but then I noticed that it seemed to be skipping.
I decided to let it go and at one point my print bed went to high or something because the head dug into the bead and tore the plastic off the the top.
A great deal of pressure was put on the extruder head and I think it might be bent.
Maybe it was like that before, I can't really say.
For my first problem, Is my extruder head clogged?
Is there a way to clean it?
I'll get some pics when my cell phone charges.
Any help would be appreciated... I'm having a very bad time with the SD3.