So, I am trying to make a mold using ABS filament in da vinci 2.0/2.0 XYZ printer.
I am constantly having an issue with filament not sticking properly to the bed. When the printer tries to fill, it then dislodges other printed sample too (see in red).
Can someone advise me where I am having an issue ?

Thank you
Sushil

#3D printing #printing for the first time

2

Re: Da vinci 2.0 Filament not sticking to the bed

ABS filament shrinks as it cools, leading to warping and lifting at the corners or complete detachment.Turn off part cooling fans for the first few layers (or completely for ABS if possible).