Topic: The Best Mod ever for any XYZ Printer
I have had the Da'vinci 2.0 for 5 or 6 years. When I first got it worked almost flawlessly. However, I never felt the quality was what I expected and the limitations and difficulty of ABS became problematic. I stopped using it until recently. When I went to use it again the printer did not move on the Y axis. I sent a request for support to xyz priming on 4/24/2020, which as of yet they have not responded. With the help of a friend I fixed the initial problem. Then uploaded the Repetier software, which was an improvement. Then I ran into problems with the extruder 2 not feeding. Which after trying solutions online I could not fix it. Then while cleaning the hot end I broke one of the wires connecting to the extruder 1.
The replacement hot- end was around 170.00 which would not fix the problem with extruder 2. Finally I came up with the following "mod". Which I am now happy to say I am getting the best prints I have ever got.
If some is interested in how I modded the case I will be glad to in another post.