1

Topic: Checking moisture in filament ?

I would like your honest opinion. If i take a piece of Bowden tube about 3 feet long and seal a humidity probe in one end  would it read the amount of moisture in the filament when inserted into the tube?

Thanks
Dale

Ultimaker S3.

2

Re: Checking moisture in filament ?

probably not

SD4 #1 & #2 - Lawsy carriages, E3D v6, Rumba controller board, mirror bed plate, X motor fan, upgraded PSU & Mica bed heater
SD4 #3 - in the works ~ Folgertech FT-5, rev 1
Printit Industries Beta Tester - Horizon H1

3

Re: Checking moisture in filament ?

Most likely not, as the humidity has soaked in to the filament. The only way is to assume there is humidity in it and dry it. I make it a practice to dry every spool a minimum of 12 hours before use. Even new spools that where sealed as I have had new sealed spools have moisture in them as well. I don't want to run out mid print and put on a new spool only to find out it has moisture in it and now my print looks like a sponge.

Printing since 2009 and still love it!
Anycubic 4MAX best $225 ever invested.
Voxelabs Proxima SLA. 6 inch 2k Mono LCD.
Anycubic Predator, massive Delta machine. 450 x 370 print envelope.

4

Re: Checking moisture in filament ?

simply put, if it is out in the open, it is absorbing moisture. period. there is no getting around that.

places with high humidity (Florida) are going to be worse than places with low humidity (southern Arizona), but the filament will absorb moisture regardless - just a matter of how much and how quickly.

SD4 #1 & #2 - Lawsy carriages, E3D v6, Rumba controller board, mirror bed plate, X motor fan, upgraded PSU & Mica bed heater
SD4 #3 - in the works ~ Folgertech FT-5, rev 1
Printit Industries Beta Tester - Horizon H1

5

Re: Checking moisture in filament ?

I agree with user "heartless"'s opinion: The filaments will inevitably absorb moisture, and their placement doesn’t really make a difference. It's best to use them with a filament dryer, or if you're as lazy as I am, just bake them in the oven before use.