hi there,
i was wondering if it would be possible to make plastic pellets by melting them in a pot and having it drip out through a nozzle into a bucket of water like how lead BBs are made as oppose to using a shredder.
You are not logged in. Please login or register.
SoliForum - 3D Printing Community → Filament → making plastic pellets
hi there,
i was wondering if it would be possible to make plastic pellets by melting them in a pot and having it drip out through a nozzle into a bucket of water like how lead BBs are made as oppose to using a shredder.
do not think it is that simple.
look here
http://www.homemadepelletmill.com/blog/ … llets.html
most plastics have a life to them. they can only be heated cycle so many times before it starts to break down. You would be better off with a shredder