Topic: Say at home order - lots of time to print but running low on filament.
I hope everyone is doing well.
With this stay at home order I have lots of time to print but running low on PETG. my machine uses 2.85mm Dia. filament so I can't get any locally and amazon is deferring orders right now (3 weeks out). living in Sunny Florida I have a lot of problems with Humidity so I never keep much on hand. I have tried plastic totes, cereal containers, Exec. but it still draws moisture.
I am thinking of designing a dehumidifying box (dryer box) that will pull and store the moisture outside the box.
Thanks