Topic: help mini maker problem
where is the problem, please help, this happens for two days .. it is calibrated, the print temperature on the PLA is 208/210, i tried to reduce and increase the temperature and always the same ..


You are not logged in. Please login or register.
SoliForum - 3D Printing Community → XYZ Printing Help/Repair/Maintenance → help mini maker problem
where is the problem, please help, this happens for two days .. it is calibrated, the print temperature on the PLA is 208/210, i tried to reduce and increase the temperature and always the same ..


Could be a clogged nozzle. Or bad filament.
i cleaned everything up and again it looks like it is filamentary while it is slow working ok it is, but while it goes a little fast to normal it gets fucked up immediately