Topic: 3D printed retro car Hotrod Pickup that was made as a gift.
Hi folks!
I just want to share my new work! I made this car as a gift to my grandfather. He is a real fan of retro car, especially Hotrod.
Highlights:
Printer Tronxy x3, HC19-carbon plastic, nozzle 0.4.
The height of the compressor layer, unit, valve covers, headlights, grille is 0.15, and the rest is 0.3.
Nozzle temperature is 230 C.
Table — 80 C.
Blowing minimum.
Free STL: https://www.thingiverse.com/thing:2465732
![]()
![]()
![]()
![]()
![]()
Process:
![]()
![]()