After receive my printer I did some pieces very well, like the cube example and other little pieces more for testing.
But recently, i am facing some problem in finish the pieces, it seems like if is cutted (i attach some photos here).
If someone can help me, will appreciate, i am newbie with this resin printers, so I am sure is something that I am doing wrong.
Some questions that I have:
a) Why in the bottom of the pool (in the plastic transparent) appears me all this cured resin? The piece that i try to do is even more little and appears cured resin in places where not must be UV light
b) Ambiental temperature can modify resin properties? I have printer in a room with window opened, so is possible be at 5-6ºC or less even. Can be this one reason? I need to put to work in a place with more temperature?
c) I try always to print pieces at 45º degrees, this is correct right?
d) Why at 70% of the piece, seems cutted and not print more?
I hope someone can give me a little hand, thanks in advance for your attention,
Happy new year and best regards!
➤ Forum: https://www.3d-work.es/foro
➤ Facebook: https://www.facebook.com/3D-Work-596165037507660
➤ Thingiverse: https://www.thingiverse.com/3D_Work