Topic: blue tape 3m brand #2090 with non heated bed
Once again, thank you all for the help. I feel i am really close to understanding things with my printer.
I read an article the other day about useing the "Magical Blue Tape" by 3m, number 2090. So i have been using that. One issue i am running into, is the fact that the PLA is sticking hardcore to the tape. It does not come off easy. I have adjusted z offset and it is, in my opinion, spot on. The PLA is not digging into the tape, just sticks to the blue tape, or any kind of masking tape like crazy. i have tried three different brands and numbersof tape haha
Usually i have to remove the tape because my putty knife destroys the tape in the process haha. Is there a better material to print PLA on? i use hatchbox and XYZ PLA.