1

Topic: Stall Protection + Autostart Wiring

Hello Everyone,

I believe I just finished assembling my Filastruder but while its already apart I'd love to get autostart working.

The instructions posted by D-Tek previously seem to be made before the stall protection board was added. I feel his solution of motor positive to pin 6 and jump pin 4 to 5 would cause the stall protection board to be bypassed.


Is it possible to get autostart working will stall protection?

Thanks,


-Blake

2

Re: Stall Protection + Autostart Wiring

I can't recommend autostart as the PID controller has no way of waiting the recommended 10 minutes before starting the motor, but if you want to do it anyway, you'd just wire the stall protection board input in place of where Dtek says to wire the motor, and then wire the motor to the stall protection board.