I agree with Carl that your layer split is due to uneven cooling. The cause of uneven cooling can be complicated since your Da vinci 2.0A is enclosed. In theory, you should not have uneven cooling if you preheat your bed long enough. Some factor can make things complicated.
1. You are printing in very cold environment such as basement in cold place.
2. You leave your printer Front or Top cover open or even have the layer cooling fan or case fan mod.
3. You open the front door or top cover in the middle of the print and suddenly bring in cold air. (I notice the split happen relatively high in top)