Topic: Glass bed clamshell chip
Da - Vinci Ai0s last night I printed a part, this morning it was complete and the bed had completely cooled, normally this releases the part easily, but this morning it was well stuck, I managed to insert a blade under the corner and seperated the part, however, an area of the glass bed lifted with the part, perhaps half a millimetre thick and about 1/2" round, the glass was still firmly attached to the part (I eventually cleaned it off with a diamond file) but this leaves me an area of the heated glass bed with a clamshell chip missing, I will try and avoid printing on that area, two questions, is the glass fixed to the heater matrix, and how easy is it to replace it?
Thanks