scobo wrote:It's very "cheap and easy" to change the slicer with a 1.0A ......... flash repetier !
Doesn't cost anything, takes 5 minutes, then you can use whatever slicer you want.
Yes, the flash itself if cheap and easy, but the calibration after that may or may not be easy depend on the skill set he have. I wound strong recommend to flash repetier-firmware if he is confident with it and he knows his hardware have no issue for sure.
If he indeed have wire harness issue and he flashed repetier-firmware, then the troubleshoot become even more complicated. It can be calibration issue, firmware configure.h issue or Cura configuration issue.
(Da Vinci 1.0, Jr. 1.0 RAMPS, miniMaker) X4, (Creality CR-10S, CR-10 mini, Ender-3) X4, Anycubic MEGA X4, Anycubic Chrion X1, ADMILAB Gantry X2 (MonoPrice Maker Select V2, Plus, Ultimate)X4--Select mini X1, Anycubic photon X4, Wanhao duplicate D7 X1.
iNSTONE Inventor Pro X2, CTC Dual X2, ANET-A8, Hictop 3DP-11, Solidoodle Press, FLSUN I3 2017X1