Topic: Nozzle temperatures for Mini W
I made test-prints on FW 1.1.2 for all (to me) known materials for Mini W. The temperature mentioned is the average reading in the Windows application.
If you want to change to 208 degrees, just change the third byte on page 08 to 5A 50 55 00.
There is a good chance that the list of supported materials has grown in later FW releases.
Temperatures PLA:
3F 193 '--' (same name in app)
40 193 '--' (same name in app)
41 203 Purple
42 203 Blue
43 203 Neon Tangerine
44 203 Viridity
45 203 Olivine
46 203 Gold
47 203 Green
48 213 Neon Green
49 203 Snow White
4A 213 Neon Yellow
4B 203 Black
4C 203 Violet
4D 203 Grape Purple
4E 203 Purpurine
4F 203 Clear Yellow
50 213 Clear Green
51 203 Clear Tangerine
52 203 Red
53 203 Cyber Yellow
54 203 Tangerine
55 208 Clear Blue
56 213 Clear Purple
57 213 White
58 203 Clear Magenta
59 203 Yellow (Clear Yellow in Android app)
5A 203 Nature
5B 193 '--' (same name in app)
5C '--' refuse to print, error msg, must make voltage reset to resume testing.