Topic: Help With DaVinci 1.0
I have my printer flashed with Repetier, and something occurred after almost a year of flawless usage.
I had a larger print running in the printer and it looks like the print ended up being too wide and the extruder ran into the rail on the left side of the printer. now when I try to get it to print something it will start the print as normal, then about 10 seconds in to the first layer, my printer head stops running its path starts heading left in a straight line to crash into wall.
What would cause this sort of thing? is my motor burned up?
Any help is greatly appreciated.