I just wanted to share a few photos of a SLA printer I have been building to add to our services offered. It still needs some minor redesign, new leadscrews, some parts need to be milled out of aluminum and the case finished. I hope to convert it to a UV LED-LCD using either a 10.1 or 12.5 inch screen and a 100-150w 395-405nm LED array. It was made using a spare chassis from our R-530 printer, leftover makerslide and just random parts I had laying around. The spare parts used influenced the whole design. The prints shown are using Makerjuice G+, now I am using FTD Snow White which is a million times better. If you are considering building a DLP printer and have any questions fire away.