1

Topic: Gliu - ABS Glue - For Heated ABS 3d Printer Beds - NO MORE GLUE STICKS

This stuff is awesome for getting your prints to stick and doesn't leave a mess like glue.

https://www.etsy.com/ShaunsShapes/listi … 0590912043

2

Re: Gliu - ABS Glue - For Heated ABS 3d Printer Beds - NO MORE GLUE STICKS

Won't this do the same thing?

https://www.amazon.com/Oatey-30922-Spec … B0069K8EUI

Ultimaker S3.

3

Re: Gliu - ABS Glue - For Heated ABS 3d Printer Beds - NO MORE GLUE STICKS

I just mix some of the leftovers and supports in a jar of acetone and use that - one drop onto the bed- spread thinly and I have not had anything come unstuck (except for some small diameter, tall parts that really did need a better orientation to print properly).

4

Re: Gliu - ABS Glue - For Heated ABS 3d Printer Beds - NO MORE GLUE STICKS

That stuff is too thick

dubbsd wrote:

Won't this do the same thing?

https://www.amazon.com/Oatey-30922-Spec … B0069K8EUI

5 (edited by Kronikabuse 2017-07-21 11:38:04)

Re: Gliu - ABS Glue - For Heated ABS 3d Printer Beds - NO MORE GLUE STICKS

I'd love to see the safety data sheet for this chemical compound

Sd4 #9080 with a glass bed. E3d chimera duel extruder. Paste extruder , duet wifi.
Lawsy carriages. linear bearings. Y axis direct drive, Kinect scanner
SD4#8188 glass bed, lawsly carriages, E3d v6, octoprint http://www.ustream.tv/channel/hotrod96z28
Filastruder/filawinder, Custom Delta 300mm x 600mm

6 (edited by shaunsshapes 2017-07-21 12:44:09)

Re: Gliu - ABS Glue - For Heated ABS 3d Printer Beds - NO MORE GLUE STICKS

MSDS = Will melt your face off. lol