1

Topic: Filament loads just fine, but then...

...Sometimes the print is fine, and sometimes it just stops advancing the filament at random times. I've removed and cleaned the head repeatedly and it doesn't happen on every print. Small items usually print no problem. But on larger prints that say it'll take several hours, I'll come in about an hour or two into the print and there will either be a small section, large-ish section with chunks missing, or just a big ball of goo...

Help!

2

Re: Filament loads just fine, but then...

May try printing at a higher temp. There are many variables that could be the cause. Might look at the temp profile and see what it looked like and if it was stable through out.

Printing since 2009 and still love it!
Anycubic 4MAX best $225 ever invested.
Voxelabs Proxima SLA. 6 inch 2k Mono LCD.
Anycubic Predator, massive Delta machine. 450 x 370 print envelope.