1 (edited by zoe 2017-07-11 03:20:13)

Topic: Dual Extruder 3D Printer, surface smooth as single nozzle printed

Hi everyone,
I'm Zoe from Yite ET 3d printer.

Yite Tech China, a professional 3d printer manufacturer for more than 3 years with strong R&D Team, focusing on 3d printer only.
We manufacture 3d printers for other suppliers on alibaba and supply 3d printer sold on Amazon / 3dprintersonlinestore/ LAZADA   and other shopping website.

ET-C1 is a dual extruder 3d printer we manufactured with excellent print quality.
Each printer will be  precisely aligned by Proficient workers before sent out.
This is the link on Alibaba.
https://www.alibaba.com/product-detail/ … .43.BePYib

Comparing with other dual extruder 3d printer,
The advantages of ET-C1 are as below.

1.We use Thicken metal plate unibody structure, not assembled parts gantry,  It's not only with longer lifespam,  but also reduce vibration when printing, thus improve the print quality.

2.Dual Extruders optional.  Precisely aligned at factory by proficient workers.
   So you can print in two nozzles and get smooth surface like one nozzle printed.

3.Moreover, it's fully closed to insulate, Can print high temp filaments perfectly.
   compatible with PLA/ABS/Wood/TPU/HIPS/PETG/PVA/Carbon Fiber etc.,

4.Even on the top we use metal structure+arcrylic, so it's more compact, no hump on the top like QIDI,Flashforge.

5.Larger build volume, 290x200x200 for single nozzle, 230x200x200mm for dual nozzle.

Sale price :
Single extruder $620
Dual extruder $652
(not include shipping and import tax duty)
Price will be lower in large quantity.

Please contact me for more details.
WhatsApp  +86 18676730349 
Skype/Email  [email protected]

Zoe

http://soliforum.com/i/?CVlYPoB.jpg
http://soliforum.com/i/?QPoOIcw.jpg

http://soliforum.com/i/?OwqBYv9.jpg

WhatApp +86 1867 6730 349
Skype [email protected]

2

Re: Dual Extruder 3D Printer, surface smooth as single nozzle printed

Basically the same post you made before

Sd4 #9080 with a glass bed. E3d chimera duel extruder. Paste extruder , duet wifi.
Lawsy carriages. linear bearings. Y axis direct drive, Kinect scanner
SD4#8188 glass bed, lawsly carriages, E3d v6, octoprint http://www.ustream.tv/channel/hotrod96z28
Filastruder/filawinder, Custom Delta 300mm x 600mm

3

Re: Dual Extruder 3D Printer, surface smooth as single nozzle printed

Just a note to your research team. Don't claim you can print carbon fiber if you have brass nozzles. Yes you can print it, but your nozzles will be destroyed and worn out within a few prints. For carbon fiber you need hard metals nozzles like stainless steel.

Printing since 2009 and still love it!
Anycubic 4MAX best $225 ever invested.
Voxelabs Proxima SLA. 6 inch 2k Mono LCD.
Anycubic Predator, massive Delta machine. 450 x 370 print envelope.

4

Re: Dual Extruder 3D Printer, surface smooth as single nozzle printed

Kronikabuse wrote:

Basically the same post you made before

Hi Kronikabuse,
Thank you for your reply.
They are two different model.

WhatApp +86 1867 6730 349
Skype [email protected]

5

Re: Dual Extruder 3D Printer, surface smooth as single nozzle printed

carl_m1968 wrote:

Just a note to your research team. Don't claim you can print carbon fiber if you have brass nozzles. Yes you can print it, but your nozzles will be destroyed and worn out within a few prints. For carbon fiber you need hard metals nozzles like stainless steel.

Hi Carl,
Thank you again. ^_^
There is a nozzle kit included for free. Customer can choose brass or stainless steel.

Zoe

WhatApp +86 1867 6730 349
Skype [email protected]

6

Re: Dual Extruder 3D Printer, surface smooth as single nozzle printed

Oh I see. You should send me on to test out. I'll do a nice write up and put it through its paces

Sd4 #9080 with a glass bed. E3d chimera duel extruder. Paste extruder , duet wifi.
Lawsy carriages. linear bearings. Y axis direct drive, Kinect scanner
SD4#8188 glass bed, lawsly carriages, E3d v6, octoprint http://www.ustream.tv/channel/hotrod96z28
Filastruder/filawinder, Custom Delta 300mm x 600mm

7

Re: Dual Extruder 3D Printer, surface smooth as single nozzle printed

Yea, please show some samples up!

8

Re: Dual Extruder 3D Printer, surface smooth as single nozzle printed

AOYOU3D wrote:

Yea, please show some samples up!

Hi AOYOU3D,
Thank you for your reply. I'll post some printed model for your reference. ^^

Zoe

WhatApp +86 1867 6730 349
Skype [email protected]

9

Re: Dual Extruder 3D Printer, surface smooth as single nozzle printed

NEW EXTERIOR! DAUL EXTRUDER 3D PRINTER!
Full metal structure, fully closed

Please contact me if you're interested. Thanks. Zoe

http://soliforum.com/i/?PIC0aVB.jpg

WhatApp +86 1867 6730 349
Skype [email protected]

10

Re: Dual Extruder 3D Printer, surface smooth as single nozzle printed

http://soliforum.com/i/?oGUQIKq.jpg

WhatApp +86 1867 6730 349
Skype [email protected]