cgrillo wrote:Cheers, something else must have happened to this card!
Mine was broken for pulling magnet fields from some neodymium rare earth magnets. I think that the part who broke was the antenna because:
* I wasn't able to read the TAG at anytime, most times the card was not recognized by the reader, been trying to read for 10 minutes and nothing, but after hours i tried again and after a couple tries the TAG becomes recognized.
* If the card gets recognized, you can see that the data is still the same, also you can write and read, but if i move the TAG out the reader antenna and try to read again, then i can have recognition problems again.
Sooo, people, don't try stupid things with magnets as i've done. ;P
s.ogorman wrote:Ok I will send you my address by PM and we can see if it works. if it does I will send you my tag in return 
Cool mate, i'm very interested in know this behaviour, please keep us informed on this test.
Cheers & Regards,
CoolArts
XYZ Junior/Mini Passwords Thread
If you are in a hurry and need your password NOW, or if it takes me too long for you, you can read the posts from 1851. I'm not going to be as effective as Bozo or Cgrillo, but you can give a try with me. If PASSWORDS thread follow it's current flow: asking for repeated passwords, not returning or false PACKS... I will end up with it as others before me.