1

Topic: Makerbot filament

Hello all,

I just want to ask if anybody has used Makerbots 1.8mm filament on a solidoodle 2?

I'm having problem printing with the filament. any suggestions on settings that I should tweek?

it seems to have a problem extruding, as the raft fails to stick or uneven deposit.