Topic: PLA coming out way to thin
I've had my filastruder and winder sins last December and have worked with it on and off sins then. I built it, didn't touch it for a while, then made the included abs and it went well and now a few months from that I tried making pla. I extruded at 180 for a little bit to purge any remaining abs and it was very thins so I started going down 5-10 degrees at a time until I go to a 100 at with point the motor slowed to a stop and I turned it off, the max width I go was 2mm when it stalled but before that a 110 it was 1.2. the dehumidifier in the closets of my basement where running on high and continues, they said 40% humidity(in the closet) but my throat felt like it was lower(in the main basement).
the barrel was full and had a the funnel section of a water bottle filled too. The pellets are from filabot and I have notice that they are round and maybe a little bigger than the abs pellets around 3-4mm but the page says 5mm is the max so they are in spec.
no fan
the tower came first when it was clamped nozzle down to my desk, the nozzle was about a foot from the ground
http://imgur.com/a/tyusz