The form bot T rex appears to be a large scale Prusa I3 variant.
My impressions on this printer seems like a heap of money . but it is big .
IIRC the larges I have seen on the market.
Carbon fiber enforced and fiberglass enforced nylons can be printed in any printer capable of high temps
I would caution you on a few things here. Understand the laws of scaling . So you are going to print a 8" cube a print that size is going to take a long time. to print a 16" cube is NOT twice the size it is 8 times the size . so for sake of argument if the 8" cube is a 24 hour print the 16 in cube is a 8 day print.
the heat bed will draw a bit of power 4 times that of 200 x 200 bed plate.
IMHO abs prints on that printer will likely be a challenge for ABS prints that large you likely need an enclosed heated chamber.
Also in a printer that big , especially the dual head version you are going to get a lot of vibration that head moving back and forth and the print bed moving oscillating with a large print you are accelerating lots of mass over and over again. so it may shake a bit.
dual extruders are nice and do not just think dual color. you can use dissolvable support or print flexible and stiff material in the same part. .
IMHO that size printer is starting to stretch the laws of physics and the design limits of the prusa design..
IMHO if i were to buy a large printer Iwould likely buy this one https://folgertech.com/products/folger … rinter-kit
Tin
Soliddoodle 4 stock w glass bed------Folger Tech Prusa 2020 upgraded to and titan /aero extruder mirror bed
FT5 with titan/ E3D Aero------MP mini select w glass bed
MP Utimate maker pro-W bondtech extruder
Marlin/Repetier Host/ Slic3r and Cura