1

Topic: Stepper Motor clicking on single color spool

I am a new Da Vinci Jr owner.  have gone through a Black spool and most of a clear - printing and learning.  No issues and I get good prints for the most part (do get some garbage - but that is usually my issues and needing to clean support better).

Yesterday I loaded a clear yellow spool.  Started an overnight print of an object that would take up the full bed.  Overnight I could hear the stepper motor clicking.  I had heard this ocassionally on the other rolls but saw no obvious ill affects and simply "logged it" as a possible need to check the X and Z axes.  But it didn't seem to be consistent or an issue.

Anyway, I woke this morning to a non-print and just garbage on the bed.  Tried to print something else and noticed it was not laying down right.  Tried again this evening on a small item and same thing - clicking steppter and gaps in the print.

Switched back to clear - and nada - no clicking and a good print.

I cannot find a direct correlation thread anywhere so figured I'd post and see if anyone had any thoughts.  At this point I'm wondering if this roll of clear yellow might be too large?

Thanks

2

Re: Stepper Motor clicking on single color spool

You just got a bad spool. I have three that just wont feed or print no matter what do. It just happens sometimes and come with the hobby.

Printing since 2009 and still love it!
Anycubic 4MAX best $225 ever invested.
Voxelabs Proxima SLA. 6 inch 2k Mono LCD.
Anycubic Predator, massive Delta machine. 450 x 370 print envelope.

3

Re: Stepper Motor clicking on single color spool

Interesting response - and not one I was expecting smile

After my original post I pulled out my Clear Yellow and reinserted my clear.  I printed a 1/10th scale cooler, lid and drum.  Some minor clicking but it was only in two spots - when originally laid down and then once mid-print.  On a whim (after reading a post about the tension lever on a 1.0 being too tight) I pulled back on the lever as if loading and heard an audible "click" - after that no more clicking.

The clear printed all three objects perfectly without issue.

This morning after reading your post I took the calipers to my spools - Black was 1.68, clear was 1.66 and the Clear Yellow was 1.57.  Certainly seems to be off on size.

This morning I'm going to try one more time with yellow and if it clicks relegate it to the "bin" and simply get another spool and see what happens.

Thank you again for the quick response.

4

Re: Stepper Motor clicking on single color spool

Ok disregard the m easurements  I wasn't awake.  I retook the measurements down the filament away from what had been in the feed and all three spools measure at 1.75.

The yellow is again clicking this morning - so it seems even more likely your explanation is right.  There is something "wrong" with this spool for whatever reason.