Topic: Faults in the print from the STL file or XYZware
Hi,
I've been using an xyz Davinci Junior for a while now and very happy with the prints apart from a small issue with my last project.
In the first picture this was the print from xyzware after slicing, I contacted support about the "fault line" in the print to see if I could do anything, they recommended putting it through an STL fixer which I did, that gave me the second image.
The third image is one I've done in black and I must say it looks fantastic .... except for the fault!
Anyway anyone any suggestions or is it just poor slicing software from xyz, I tried slic3r and it looks fine but of course I can't print it!!!