Topic: S3D + Repetier = Bad Day
I was having issues with gaps in between parameter and infill in a print using Simplify3D, I had tried higher infill, slower speed, setting the extrusion to 150% and still the same thing. ssauntson recommended I check the stepper since I was using a different one. I marked 100mm of filament and told S3D it to extrude 100mm. It only extruded approx 94mm, we thought we should adjust the steps in the firmware so we increased to 510, it extruded the exact same amount. So with that I tried Repetier Host and it over extruded by approx 6mm. I reset configuration.h to original value, extruded with Repetier Host and it was almost dead on with 100mm.
Why would Simplify3D not extrude the correct amount? I have also created a ticket over with S3D but was wondering if anyone had any ideas. Can someone else try the same test with Simplify3D?
Simplify3D Print
Repetier Host Print
STL files