26

Re: Upgrading Filastruder

Tim,

Would this be OK for the 15v 5A PSU for the heater?  I need more power for nylon.

http://www.amazon.com/PC247-Satellite-i … wer+supply

27

Re: Upgrading Filastruder

Looks like it would do OK.