1

Topic: What happened to my y axis belt, and how to fix?

I left a print going overnight, and woke up to find this...

http://imgur.com/sF6MsW1

What happened? and how can I fix this? the belt is torn/melted/whatever it is right on the text that tells me what kind of belt it is, so I can't even try replacing it until i figure out what type of belt exactly it is. It's for the Y axis....can anyone help me out?

Davinci 1.0a.

2

Re: What happened to my y axis belt, and how to fix?

i bet the print head snagged on something or got bound up and it snapped

Sd4 #9080 with a glass bed. E3d chimera duel extruder. Paste extruder , duet wifi.
Lawsy carriages. linear bearings. Y axis direct drive, Kinect scanner
SD4#8188 glass bed, lawsly carriages, E3d v6, octoprint http://www.ustream.tv/channel/hotrod96z28
Filastruder/filawinder, Custom Delta 300mm x 600mm

3

Re: What happened to my y axis belt, and how to fix?

Okay I've talked with the company and it sounds like they are going to ship me a replacement belt, any resources or guides on how I can do this without screwing up my printer?

4

Re: What happened to my y axis belt, and how to fix?

Dispensergoeshere wrote:

Okay I've talked with the company and it sounds like they are going to ship me a replacement belt, any resources or guides on how I can do this without screwing up my printer?

Resources or guides? Man you learn by taking apart, take pictures if necessary and then put back together..

Seriously though get on Youtube and search. There is video for nearly everything you would need to do to this printer now..

Printing since 2009 and still love it!
Anycubic 4MAX best $225 ever invested.
Voxelabs Proxima SLA. 6 inch 2k Mono LCD.
Anycubic Predator, massive Delta machine. 450 x 370 print envelope.