1

Topic: 3D printing with fiberglass

I'm looking for a way to build a 3D printer with fiberglass printing capability such as Markforged Mark One. I haven't seen any alternatives to that one, so I was wondering if there are any extruders out there that support fiberglass printing at all? Ideally I would order a kit and then modify it in a way to add additional extruder for fiberglass, but I'm not sure what option would be the most viable. Any advice would be greatly appreciated.

2

Re: 3D printing with fiberglass

The mark I is an unusual approach to 3d printing.

The alternative is a regular FFF/FDM printer with carbon fiber or fiberglass fill.
The caveat is you need a good quality hot end like an ed3 and a hardened nozzle as hard metal fills, glss and cf tend to be abrasive and wear out nozzles.

3Dom USA sells Engineering grade fiberglass reinforced PLA. And several vendors /manufacturers offer high performance carbon fiber  filament. 

https://printedsolid.com/collections/carbon-fiber
http://www.3domusa.com/glass-filled-pla/
I hope this helps
tin

Soliddoodle 4 stock w glass bed------Folger Tech Prusa 2020 upgraded to and titan /aero extruder mirror bed
FT5 with titan/ E3D Aero------MP mini select w glass bed
MP Utimate maker pro-W bondtech extruder
Marlin/Repetier Host/ Slic3r and Cura

3

Re: 3D printing with fiberglass

Actually my approach would be unusual as well, basically very similar than the one that is used in Mark I since I have very specific needs. So I intend to place fiberglass into FFF/FDM printed model just the same way as Mark I does. Do they use a special extruder for fiberglass?