1 (edited by jwalker55 2016-01-25 22:38:38)

Topic: Z banding (Da Vinci Jr 1.0w)

One thing I've noticed on pretty much all of my prints since getting my printer a couple months ago is z banding (see attached pics).  Any clues as to what would be causing this?  It looks almost like it matches the thread pitch of the threaded rod, but I can't visually see any wobbling or anything that looks off, and the threaded rod looks like it's plenty lubricated.  Is this just standard print quality for the Jr?

Post's attachments

20160124_191746_HDR.jpg
20160124_191746_HDR.jpg 2.07 mb, file has never been downloaded. 

20160125_172220_HDR.jpg 3.72 mb, file has never been downloaded. 

You don't have the permssions to download the attachments of this post.

2

Re: Z banding (Da Vinci Jr 1.0w)

getting the same quality on standard quality print. guess that's just the jr's quality. I'm getting to regret this purchase. having far better quality and speed with the 3d Up Mini...