1

Topic: Print not center. How??

My prints out of noware prints off center now. Can figure out why or how to fix. Anyone have this issue?

2

Re: Print not center. How??

zoeconner wrote:

My prints out of noware prints off center now. Can figure out why or how to fix. Anyone have this issue?


Because you have a dump area which is included in the bed dimensions you have to alter the bed dimensions in your host so that it is centered. Your bed is not really 210 by 210. I think that is what the bed area is.. You have to include the distance from the home position across to the end of the X travel then find the center of that..

Printing since 2009 and still love it!
Anycubic 4MAX best $225 ever invested.
Voxelabs Proxima SLA. 6 inch 2k Mono LCD.
Anycubic Predator, massive Delta machine. 450 x 370 print envelope.

3

Re: Print not center. How??

So should I choose bed with dump bed in settings?

4

Re: Print not center. How??

No, just play with the bed dimensions until it starts in the center. You can measure with a ruler from to the far side of the bed then divide that in half and get close. Same process for the Y axis as well.

Printing since 2009 and still love it!
Anycubic 4MAX best $225 ever invested.
Voxelabs Proxima SLA. 6 inch 2k Mono LCD.
Anycubic Predator, massive Delta machine. 450 x 370 print envelope.